5% intermediate depth为3.8mm如何理解,前提是工件在淬火后根据从外到里组织来对工件进行深度的测定 我们做过5%ITP的,用100倍目测,在视野中非马占5%的深度 We check the depth of 5% ITP(Intermediate Transformation Products).
You may evaluate 5% ITP depth by metallographic photo.
Here I have some ,you may reference.
Note:figure1 to figure 6ITP% content :<1%; 1%;5%;10%; 20%;50%.