LucySun 发表于 2018-12-28 09:31:18

What kind of preparation need to do for Nadcap Audit ?

Dears

       Would you like to share your experence that if we change the instrument type from A to B,
      what kind of preparation shall we do for the Nadcap audit?
      What potential riks will we have to face?

Thanks very much in advance for your sharing.

BRs
Lucy
      

hackyue 发表于 2019-4-23 14:16:26

Review the difference between type A and B firstly.
Analyse the risk if you replace A by B.
Produce some batch parts and check the property. If OK, do it.

maike 发表于 2019-6-23 13:03:49

From my side, it's improvement that you change instrument from A to B.
And analyze the result , compare the risk of A and B.
last do the test and analyze the result.

z051443019 发表于 2019-7-18 13:36:24

You should consult some certification experts