不似天才 发表于 2021-3-8 16:09:47

AMS 2750F About calibration accuracy of sensor

Hello everybody, i have a questionabout calibration accuracy of sensor as below,
According to AMS 2750F table 1,if the calibration accuracy of the type S control sensor is exceed the ±0.6℃ or±0.1%,
shall we scrap the sensor or continue to use the sensor with correction factors?
Hope your answer!

山腰樵夫 发表于 2021-4-9 13:14:18

You shall use the sensor with correction factor. see table1 note(9).

LucySun 发表于 2021-4-15 09:32:02

In my opinion, we have to scrap these sensors becuase they can't mee the requirements.

For table 1 Note 9
I think it is only suitable for sensors type not listed in Table 1 and used above 1316℃ then we can follow up the rules of Note 9.

随缘吧 发表于 2021-6-21 11:19:43

See table1 note(9).....