不似天才 发表于 2021-3-8 16:14:03

AMS 2750F what is Analog instrument?

what is Analog instrument?
Could you give me an example with picture,thanks!

LucySun 发表于 2021-4-14 15:54:44

In order to know what is an anolog instrument maybe you can refer to 2.2.19

2.2.19 Digital instrument
An instrument that records process measurements in a digital (numeric) display format, or an instrument that prints both the scale (graph) and trend line simultaneously.
A recorder trend line on pre-printed pater is an anolog record.
页: [1]
查看完整版本: AMS 2750F what is Analog instrument?