what is the Tevo Test
I meet a difficulty today-TEVO TEST从来没听过这个试验,哪位坛友给讲一讲?先谢谢了. Material sorting
Tevo test
Foster,Germany it is a method to test on the finished surface , without breaking the part 回复 3# 察哈尔汗
is it means thats a method OF NDT 回复 4# heatingsun
Yes.
It is an instrument for NDT.
There are 2 suits in my lab now, but I can't talk more about it,
Reasons, I think you know. 回复 5# 察哈尔汗
i got it Timken always have some strange but precision equipments. Maybe it's some kind of NDT method he can do everything,能够知道材料是否混料,渗层是否足够,硬度是否合格,磨削是否烧伤....
这是一种根据材料内部结构不同,从而电导率也不同的原理开发出的一个很神奇的仪器。
但只能定性,无法定量。使用这个仪器的公司很少,需要积累大量数据才能发挥其作用。
回顾自己一些帖子,有很多没有结论的,自己来补下答案。
又算填了一个坑。:) TEVO是TIMKEN一款热电分析仪,分析渗碳层的。 冷艳锯 发表于 2017-11-16 11:14
TEVO是TIMKEN一款热电分析仪,分析渗碳层的。
it is not only for case depth, it knows everything.
material mix, case, hardness, grind burning...... BYW: Does Timken set up or only use this kind of test method?