watereast 发表于 2010-3-16 15:16:40

STAINLESS-stainless steels and their properties

本帖最后由 watereast 于 2010-3-16 15:46 编辑

STAINLESS
- stainless steels and their properties
Table of Contents
Introduction .....................................................................................................................................................3
Use of stainless steel ..............................................................................................................................3
How it all started ..................................................................................................................................4
Stainless steel categories and grades..................................................................................................................5
The effects of the alloying elements........................................................................................................5
Corrosion and corrosion properties ...................................................................................................................9
PASSIVITY.............................................................................................................................................9
AQUEOUS CORROSION.........................................................................................................................10
General corrosion.........................................................................................................................10
Pitting and crevice corrosion.........................................................................................................11
Stress corrosion cracking ..............................................................................................................14
Intergranular corrosion..................................................................................................................16
Galvanic corrosion.......................................................................................................................18
HIGH TEMPERATURE CORROSION ..........................................................................................................19
Oxidation.....................................................................................................................................19
Sulphur attack (Sulphidation).......................................................................................................20
Carbon pick-up (Carburization).....................................................................................................21
Nitrogen pick-up (Nitridation).......................................................................................................21
Mechanical properties ....................................................................................................................................23
Room temperature properties...............................................................................................................23
The effect of cold work........................................................................................................................27
Toughness ..........................................................................................................................................27
Fatigue properties ...............................................................................................................................29
High temperature mechanical properties...............................................................................................30
Precipitation and embrittlement .......................................................................................................................32
475°C embrittlement ............................................................................................................................32
Carbide and nitride precipitation ..........................................................................................................32
Intermetallic phases.............................................................................................................................32
Physical properties .........................................................................................................................................34
Property relationships for stainless steels .........................................................................................................36
Martensitic and martensitic-austenitic steels .........................................................................................36
Ferritic steels ......................................................................................................................................36
Ferritic-Austenitic (Duplex) steels........................................................................................................37
Austenitic steels ..................................................................................................................................37
References .....................................................................................................................................................38
Attachment: US, British and European standards on stainless steels..........…………………………41

yao0452 发表于 2010-12-19 18:35:43

看一下。。。。。

tyw339214511 发表于 2013-2-17 08:53:08

好东西,收藏了               

chenze2008 发表于 2013-2-18 08:35:30

好资料,已加分!

njxwl 发表于 2013-5-23 16:42:07

好东西,收藏了,正好有用

cjzhou 发表于 2013-12-14 02:45:24

谢谢分享                                                                     

bbsfhb 发表于 2015-11-21 21:36:16

英文书籍不好找,好的学习材料

shihuan211152 发表于 2017-12-26 09:35:51

thanks for sharing . i just want to set up an internal material depot , so this works for me.

小杰 发表于 2021-7-16 09:31:37

感谢楼主分享~好东西,学习了

hhandi 发表于 2021-7-20 10:05:25

感谢楼主分享,先顶一下。

yuwen 发表于 2021-9-11 17:37:49

stainless steels and their properties
页: [1]
查看完整版本: STAINLESS-stainless steels and their properties