GCr15 Anomaly microstructure
Please help me to analysis the root cause.http://www.rclbbs.com/viewthread.php?tid=65888&extra=page%3D1 本帖最后由 leomet 于 2010-10-16 05:12 编辑
GCr15 abnomal microstructure
It looks like a layer of fresh Martensite .