realstone 发表于 2012-2-18 22:06:45

heat treatment HRC55 ?

The drawing indicated " heat treatment HRC55"
是指整体达到这个硬度还是表面达到
整体热处理和表面热处理用英语怎么说

kop123 发表于 2012-2-19 05:44:37

本帖最后由 孤鸿踏雪 于 2012-2-19 10:16 编辑

图面显示为HRC55.整体热处理:bulk heattreatment;表面热处理:surface heat treatment。

zhengcj 发表于 2012-2-20 12:55:10

Can you specify what kind of heat treatment used by the part? Is there any requirements in the drawing?

Normally, if not specified specially, the hardness requirement in the drawing means the surface hardness.

We can use "direct hardening" for "整体热处理“, and "Surface hardening" for the "表面热处理".

tangjincai 发表于 2012-2-23 15:00:50

zhengcj 发表于 2012-2-20 12:55 static/image/common/back.gif
Can you specify what kind of heat treatment used by the part? Is there any requirements in the drawi ...

不明白,英语太差,请老师说明白一点

realstone 发表于 2012-3-1 16:24:43

No other requirements in the drawing!
Only indicated Heat treatment HRC55+- 3