Please help me to translate this paragraph:
“In common commercial practice, an endothermic or purified exothermic gas is used as the carrier, and it is enriched with one of the hydrocarbon gases. The ratio of carrier gas to hydrocarbon gas varies widely in industry but is usually in the range of 8-to -1 to 30-to-1. the ratio used depends on the types of carrier and hydrocarbon gases, the furnace size and condition, the amount of circulation, and the surface area of the workpieces.” |
|