When I read the AMS-2750E, I found in this specification, it's absent for the temperature selection for a SAT.
For the calibration of Sensors, it stated that the temperature interval shall not greater than 140C within the measurement range.
For the calibration of instrument, it stated that at lease 3 point for equipment sensor, minimum, maximum and middle 1/3.
For the TUS, it stated that the temperature for survey shall be maximum, minimum and temperatures makes the difference between test temperatures not greater than 335C.
But for SAT, it stated no temperature for test?

do you guys have any comments on this?

签到天数: 124 天

[LV.7]常住居民III

 楼主| 发表于 2018-6-11 16:11:52 | 显示全部楼层
sorry for ignored the content in AMS-2750E.
The AMS-2750E actually stated the temperature requirement:
3.4.5.1 The displayed temperature indication and/or recording of the sensor being tested as used in production, with appropriate offsets or correction factors, at any operating temperature, shall be compared with the corrected temperature indication of the test sensor on a test instrument.

In this clause, it shows that it already gave the temperature requirement for SAT.

Thanks and for your information.
回复 支持 反对

使用道具 举报

签到天数: 248 天

[LV.8]以坛为家I

发表于 2018-6-25 17:55:51 | 显示全部楼层
I think you have got the answer by yourslf- at any operating temperature.
It makes no sense if not at the operating temperature.
回复 支持 反对

使用道具 举报

签到天数: 9 天

[LV.3]偶尔看看II

发表于 2018-10-17 14:47:10 | 显示全部楼层
Ha.
Usually, the people select one temperature he ofen used to perform SAT.
回复 支持 反对

使用道具 举报

您需要登录后才可以回帖 登录 | 注册

本版积分规则

苏州工业园区热海热处理设备有限公司 热处理论坛合作伙伴广告位 苏州出兴自动化设备有限公司

QQ|Archiver|手机版|小黑屋|热处理论坛 ( 苏ICP备11036679号 公安机关备案号:32059002001695 )

GMT+8, 2020-3-28 21:47 , Processed in 0.041744 second(s), 20 queries .

Powered by Discuz! X3.4

Copyright © 2001-2020, Tencent Cloud.

快速回复 返回顶部 返回列表